Back to Outdoors

Mortar Mixes for Garden Walls Explained

Mortar Mixes for Garden Walls Explained
DIY Guides Editorial 27 June 2026

Mortar is the part of a wall most often mixed by eye and most often mixed too strong, which causes more damage than a weak mix ever does.

What mortar is for

It beds the units so loads spread evenly, rather than brick touching brick at high points.

It keeps water out of the joints.

It accommodates small movement, which is why mortar should always be weaker than the units it bonds.

A strong cement mortar with a soft brick means the brick face fails instead of the joint. Cracks run through the bricks rather than the mortar, and the repair is far worse.

The standard mixes

Proportions are given as cement to lime to sand, by volume.

Above the damp proof course, general garden walling: 1 cement : 1 lime : 6 sand. This is the usual choice for ordinary bricks in a normal situation.

Below the damp proof course, and for copings and exposed work: 1 cement : half lime : 4 sand. Stronger, because it is wetter and more exposed.

Where lime is not used, roughly equivalent cement and sand mixes are 1:5 or 1:6 above the damp course and 1:4 below, with a plasticiser added.

Very soft or handmade bricks, and old lime built walls, want something weaker again, frequently a lime only mortar.

Why lime is worth using

Lime makes mortar more workable, so it spreads and beds easily without excess water.

It allows a small amount of movement without cracking, and it has a mild self healing effect on hairline cracks.

It holds water better, which helps the mortar cure rather than being sucked dry by the bricks.

It is more breathable, which matters on older masonry.

Hydrated lime from a bag is straightforward to use and mixes in like cement.

Plasticisers

A plasticiser entrains air, improving workability and frost resistance, and it is the common alternative to lime.

Use a proper mortar plasticiser rather than washing up liquid, which is a persistent piece of folklore. Detergent entrains air uncontrollably, weakens the mortar and can affect the set.

Follow the dose on the container. More is not better and over-plasticised mortar is weak.

Sand

Use building sand, sometimes called soft sand, for bricklaying mortar. It is fine and rounded and gives a workable mix.

Sharp sand is for concrete, screeds and bedding, and makes harsh unworkable mortar.

Sand colour varies between suppliers and between loads, and it is the main thing that determines mortar colour. Buy all the sand for a wall at once, or the joints will change colour halfway along.

Mixing consistently

Measure by volume with a bucket or a gauge box, not by shovel. Shovel loads vary enormously and every batch will differ.

Mix the dry materials first until the colour is uniform, then add water gradually.

The mortar should hold a ridge when drawn with a trowel and stay on the trowel when tipped slightly.

Too wet and it squeezes out and stains the face; too dry and it does not bond.

Mix only what you can use in around two hours.

Never add more water to mortar that has started to stiffen. Knocking it up again with fresh water destroys the set and leaves permanently weak joints.

Weather

Do not lay in frost, or when frost is forecast within twenty four hours, since freezing destroys fresh mortar.

Below about five degrees, the set slows dramatically.

In hot weather, dampen dry bricks so they do not suck the water out of the mortar before it cures, and cover new work.

Cover the top of a new wall overnight and in rain, since water running into open work washes the mortar out.

Safety

Cement and lime are strongly alkaline and cause serious burns on prolonged skin contact, which develop slowly and are easily missed.

Wear gloves, eye protection and long sleeves, and wash splashes off immediately.

Kneeling in wet mortar through trousers is a common cause of cement burns, so use a board or knee pads rather than kneeling directly in it.