Back to Outdoors

Preparing Exterior Surfaces Before Painting

Preparing Exterior Surfaces Before Painting
DIY Guides Editorial 21 June 2026

Exterior paint has to survive rain, frost, ultraviolet light and constant movement. It manages that only when it is bonded to something sound, which is entirely a matter of preparation.

Start by looking properly

Walk the whole building with a notepad before touching anything.

Look for flaking and blistering paint, cracks in render, loose pointing, rotten timber, rusting metal, blocked gutters and anything growing on the wall.

Find out why any previous coating failed, since painting over the cause repeats it. Blistering usually means moisture behind the film; flaking usually means poor adhesion or a surface that was damp.

Check for a damp source: a leaking gutter, a cracked downpipe, a bridged damp proof course or soil banked against the wall.

Fix the water problems first

This comes before any painting, not after.

Clear and repair gutters and downpipes, since a single overflowing joint keeps a strip of wall permanently wet.

Repoint failed mortar and repair cracked render.

Clear soil, planting and debris away from the base of the wall so the damp proof course is not bridged.

Allow the wall to dry out properly afterwards, which takes days rather than hours.

Washing down

Everything needs cleaning, and this is where most of the physical work sits.

Brush off loose material with a stiff brush, then wash with water and a suitable cleaner.

Treat any green growth with a fungicidal wash and let it dwell as instructed. Painting over algae seals it in and it grows through the new coating.

Rinse thoroughly and allow to dry fully.

A pressure washer is useful and easily overdone. Use a wide fan, keep your distance, and remember it drives water deep into masonry, which then needs several dry days.

Removing loose paint

Scrape back to a firm edge with a scraper or filling knife, working until nothing more lifts.

Feather the edges of the sound paint with abrasive so the join does not show through the new coat.

Where a coating is failing across a large area it has to come off completely, which is a much bigger job and worth establishing early.

Assume paint on anything built before 1980 may contain lead. Do not dry sand or burn it off. Test with a lead paint kit, and if it is present use wet methods, a chemical stripper or a specialist, and keep children and pregnant women away.

Timber

Probe suspect areas with a screwdriver. Sound timber resists; rotten timber takes the blade easily.

Cut out and splice in new timber where rot is extensive, and use a two part wood repair system for smaller areas.

Sand back to sound, clean timber and remove all dust.

Knot bare softwood with knotting solution, then prime, paying particular attention to end grain and joints.

Rake out and re-caulk the joints between frames and masonry with an exterior grade flexible sealant.

Metal

Remove rust back to bright metal with a wire brush, abrasive or a rotary wheel.

Treat any remaining rust with a converter, then prime with a metal primer suited to the substrate.

Galvanised and non-ferrous metal need a specific primer, since ordinary primers do not adhere to them.

Masonry and render

Cut out cracked and hollow render and patch with a compatible mix, allowing it to cure fully.

Fill fine cracks with an exterior filler, and use a flexible filler where movement is likely.

Test whether the surface is chalky by rubbing a hand over it. Powder on your palm means the surface is unstable and needs a stabilising solution before painting.

Very porous or newly repaired areas need a thinned first coat or a primer so the topcoat does not dry out too fast.

Masking and protection

Sheet the ground, cover planting and protect paving, since masonry paint marks permanently.

Mask windows, door furniture, vents and light fittings.

Remove or cover anything you would rather not paint around, which is usually quicker than cutting in past it.