With the sub-base compacted and the levels set, laying is methodical rather than difficult. The discipline is checking every slab as it goes down, because mortar does not wait.
Setting up
Have everything to hand before mixing: slabs stacked close by, mortar materials, a straight edge, a spirit level, a rubber mallet, spacers and a brush.
Re-check the string lines and the datum.
Lay a few slabs out dry across the area to confirm the setting out works and the cuts land where you planned.
Work from the house outwards, so the full slabs are against the building and any cuts finish at the open edge.
The mortar mix
A common bedding mix is around 5 or 6 parts sharp sand to 1 part cement, mixed to a moist consistency rather than a wet one.
The mix should hold its shape when squeezed and not slump. Too wet and slabs sink and float; too dry and it will not bond.
Use sharp sand, not building sand, which is too fine for a bedding course.
Adding a plasticiser improves workability. An SBR additive improves bond and is worth using with dense paving.
Mix only what you can lay in around half an hour, and never use mortar that has started to stiffen.
Laying the bed
Spread mortar to around 40mm thick over an area slightly larger than one slab.
Screed it roughly to the fall using a straight edge or a screed rail.
The bed must be full and continuous, supporting the whole underside of the slab with no voids.
Wet the back of porous slabs, or prime porcelain with a slurry, immediately before laying.
Bedding each slab
Lower the slab into place rather than sliding it, keeping it close to its final position.
Tap it down with a rubber mallet, working from the centre outwards, until it sits at the marked level.
Check with the spirit level in both directions, and check the fall with the straight edge against the previous row.
Check the slab is flush with its neighbours along the whole edge, since a lip of even 2mm is a trip hazard and very visible.
If a slab is low, lift it out and add mortar. Never pack underneath with chippings or try to lever it up, which leaves a void.
Joints
Use spacers to keep joints consistent, typically 8mm to 12mm for natural stone and around 5mm for porcelain.
Consistent joints are what make a patio look professionally laid, more than anything else.
Keep mortar out of the joints as you go, and brush spilled mortar off the face immediately. Cement staining on porous stone is very difficult to remove once set.
Working across the patio
Lay in rows, checking level and fall at the end of each one rather than at the end of the day.
Stand on boards laid across the slabs rather than on freshly laid paving, and ideally work backwards so you are never standing on today's work.
Leave the cut slabs at the edges until the field is complete, then measure and cut each one individually.
Curing
Keep off the paving for at least twenty four hours, and longer in cold weather.
Do not joint until the bedding has set, usually a day or two.
Protect from rain with sheeting if heavy weather is forecast before the mortar has set, and do not lay in frost or when frost is forecast overnight.
Checking before jointing
Walk the whole patio and check for any slab that rocks, which means a void beneath.
Throw water across the surface and watch it drain, looking for anywhere it stands.
Lift and relay anything that rocks or ponds now. Once the joints are filled, correcting a single slab means breaking out the pointing around it.
Safety
Cement is alkaline and causes burns on prolonged contact, so wear gloves and keep it off skin, especially at the knees.
Slabs are heavy and awkward. Use slab lifters or two people, and keep the load close to the body.