Jointing is the last stage and the one most likely to spoil good paving, because almost every product stains the surface if it is applied in the wrong conditions.
What the joint does
It stops water getting into the bedding and washing it out.
It locks the slabs together so they cannot move or rock.
It keeps weeds and ants out of the bed.
It is a substantial part of how the finished patio looks, since joints cover a surprising proportion of the surface area.
Traditional sand and cement
A stiff mix of around 3 or 4 parts sharp sand to 1 part cement, pressed into the joint with a pointing iron.
Cheap, durable, and completely unforgiving of a wet mix, which will stain porous stone permanently.
The mix should be barely damp, holding together when squeezed but not wet enough to smear.
Slow work, since every joint is filled and struck individually, and hard on the knees and back.
Keep the paving surface dry and brush off any spillage immediately, before it touches water.
Dry brush-in compounds
A dry cement based powder brushed into dry joints and then watered, or in some products left to set from atmospheric moisture.
Much quicker than hand pointing over a large area.
They work well in wider joints and need the joint to be a minimum depth, commonly 25mm or more.
Follow the instructions exactly on wetting, since too much water washes the binder out and too little leaves it uncured.
Resin based jointing
Two part epoxy or single part polymeric compounds, applied wet and worked into the joints with a squeegee and a brush, then washed off the surface.
Fast over a large area, flexible, weed resistant and strong.
Essential for porcelain, where cement based pointing does not bond to the crisp edges and cracks out.
Expensive, and unforgiving about temperature and moisture.
Most need the paving damp but with no standing water, an air temperature within a specified band, and no rain for several hours afterwards.
Residue left to cure on the surface is extremely difficult to remove, so the washing off stage is not optional and has to be done promptly.
Kiln dried sand
Used for block paving rather than slabs, brushed into narrow joints and vibrated in.
Not suitable for slab patios with wide joints, where it simply washes out.
Joint width and depth
Natural stone is usually laid with joints around 8mm to 12mm.
Porcelain is usually 5mm, since the edges are precise and wider joints look wrong.
Check the minimum joint width and depth for the product before laying the slabs, since some resin compounds will not cure properly in a narrow or shallow joint and this cannot be fixed afterwards.
Rake out any bedding mortar that has squeezed up into the joints while it is still soft.
Conditions
Do not joint in frost, in heavy rain, or in strong direct sun.
Most products specify a minimum temperature, typically around five degrees and rising, and some resins have a maximum too.
Leave the bedding to set before jointing, usually at least twenty four hours.
Check the forecast for the following day as well, since many compounds need several hours of dry weather to cure.
Protecting the paving
Test any product on an offcut or a hidden slab before committing to the whole patio.
Porous stone, particularly light coloured limestone and sandstone, picks up cement staining readily.
Work in small sections so nothing dries on the surface.
Keep a clean bucket, clean water and a sponge to hand throughout.
Afterwards
Keep off the patio for the stated curing time, usually at least a day.
Protect from rain with sheeting if weather arrives before it has set.
Check for hollow or unfilled joints once cured and make them good, since any gap becomes the point where water gets in.
Repointing later
Joints do not last forever, and pointing that has cracked out should be replaced rather than topped up.
Rake the old material out to full depth, brush the joint clean and dry, then refill with the same type of product.
Where pointing keeps failing in the same place, the slab beneath is moving, and repointing will not solve it. Lift the slab and relay it on a full bed first.