Back to Tools

Plasterboard and Plasters

Plasterboard and Plasters
DIY Guides Editorial 30 May 2026

Plasterboard and plaster are a system: the board and the plaster over it have to match, and so does the plaster to the background.

Plasterboard sizes

  • 2400 x 1200mm is standard. Also 1800 x 900mm, which is far easier to handle alone
  • 9.5mm: ceilings at close joist centres, and over existing surfaces
  • 12.5mm: the standard for walls and ceilings
  • 15mm: better acoustic and fire performance, and heavier

Edges:

  • Tapered edge: a slight recess along the long edges, so tape and jointing compound sit flush. For a taped and jointed finish that is then decorated directly
  • Square edge: for a skimmed finish, with plaster over the whole surface

Choose the edge to match the intended finish. Tapered edge under a skim coat is not a problem; square edge with a taped joint is.

Plasterboard types

  • Standard wallboard: general use, usually ivory faced
  • Moisture resistant, usually green: bathrooms, kitchens and utility rooms. Water resistant, not waterproof. Not suitable inside a shower enclosure
  • Fire resistant, usually pink or red: where a fire rating is required, such as garage ceilings, protected escape routes and around a loft conversion
  • Acoustic, usually blue and denser: for sound reduction between rooms
  • Impact resistant: hallways and high-traffic areas
  • Insulated, or thermal laminate: board bonded to rigid insulation, for internal wall insulation
  • Vapour check, foil backed: incorporating a vapour control layer

Where a drawing or the Building Regulations specify a board type, particularly fire rated, use it. It is specified for a reason and will be inspected.

Fixing plasterboard

  • Drywall screws, 32mm for 12.5mm board on timber, 38mm for 15mm
  • Screws at around 150mm centres on ceilings, 200 to 300mm on walls, and closer at edges
  • Set the head just below the surface without breaking the paper. A screw that tears the paper holds nothing
  • A dimpler bit or a drywall gun sets the depth consistently
  • Keep screws at least 10mm from a cut edge and 13mm from a bound edge
  • Stagger joints so four corners never meet at a point
  • Fix ceilings before walls, so the wall boards support the ceiling edge

Undercoat plasters

Applied to a background before the finish coat.

Bonding coat. For low suction or smooth backgrounds: concrete, engineering brick, painted surfaces. Also used to build out depth. Can be applied thicker than browning.

Browning. For high suction backgrounds: common brick, blockwork. Cheaper than bonding.

Hardwall. A modern undercoat with higher impact resistance and quicker drying. Widely used on masonry.

Renovating plaster. For walls affected by salt contamination, typically after damp. Formulated so salts do not migrate through to the surface. Essential where a wall has had rising or penetrating damp, since ordinary gypsum plaster over salt-contaminated masonry will fail repeatedly.

Lime plaster. Traditional, breathable, flexible. The correct material for older solid wall buildings, which need to manage moisture by allowing it through rather than trapping it. Cement and gypsum on an old lime-built wall traps moisture and causes damage.

Finish plasters

Multi-finish. The general purpose finish coat, over undercoat plasters and over plasterboard. The most commonly used.

Board finish. Specifically for plasterboard. Similar to multi-finish.

One-coat plaster. Undercoat and finish in one product. Convenient for small repairs, and harder to get a good finish with.

Skim is the process, not a product: a thin finish coat, typically 2 to 3mm in two passes.

Matching plaster to background

Suction is the key factor. A background that sucks water out of the plaster too fast makes it unworkable and causes cracking.

  • High suction: common brick, blockwork, old plaster. Use browning or hardwall, or control the suction with a bonding agent or by damping down
  • Low suction: concrete, engineering brick, painted or smooth surfaces. Use bonding, over a suitable primer or bonding agent
  • Plasterboard: multi-finish or board finish directly
  • Salt contaminated: renovating plaster, after fixing the damp source
  • Old solid walls: lime, to match the original construction

Mixing

  1. Always add plaster to water, never water to plaster, which produces lumps
  2. Use clean water and a clean bucket. Contamination from a previous mix accelerates the set unpredictably and dramatically
  3. Mix with a paddle in a drill to a smooth, lump-free consistency
  4. Aim for the consistency of thick cream for finish plaster
  5. Mix only what you can use in the working time, which is typically 20 to 40 minutes for finish plaster
  6. Never add water to a mix that is going off; it destroys the strength
  7. Wash tools and buckets immediately and completely

Jointing compounds

For a taped and jointed finish rather than a skim.

  • Ready-mixed jointing compound: convenient, longer working time, shrinks slightly, needs several coats
  • Setting compound, powder: sets chemically in a stated time, shrinks less, harder to sand
  • Paper tape is stronger than mesh at joints and needs bedding in compound
  • Mesh tape is self-adhesive and easier, and better suited to setting compounds
  • Feather each coat wider than the last, using progressively wider knives

New plaster and decorating

  • Let new plaster dry fully, which takes weeks rather than days. It changes from dark to a uniform pale pink
  • Apply a mist coat, emulsion thinned roughly 70:30 with water, so it soaks in and forms a key
  • Do not use PVA as a primer under paint. It forms a film the paint sits on, and it can fail later
  • Then two full coats
  • Painting fresh plaster with unthinned emulsion causes peeling

Health and handling

  • Plaster and plasterboard dust: wear an FFP3 respirator and use extraction
  • Plaster is alkaline and irritates skin. Wear gloves and rinse splashes off
  • Eye protection when mixing and when working overhead
  • A plasterboard sheet is heavy and awkward. Get help, or use smaller sheets
  • Never wash plaster or cement down a drain, where it sets. Let it settle in a bucket and bin the solids
  • Plasterboard waste must be kept separate from general waste

If it goes wrong

Plaster went off in the bucket: contaminated water or a dirty bucket.

Plaster cracking as it dries: the background suction was too high, or it was applied too thick.

Salts coming through new plaster: it needed renovating plaster, and the damp source needs fixing.

Paint peeling off new plaster: no mist coat, or PVA was used.

Screw heads tearing the paper: driven too deep. Use a dimpler bit.