Timber is sold in a system of names and numbers that is not obvious. Knowing what the terms mean prevents ordering the wrong thing.
Nominal and actual size
The size a piece of timber is called is not the size it measures.
- Nominal is the size as sawn from the log
- Actual is what you get after planing, which removes material from every face
- A piece called 50 x 100mm typically measures around 45 x 95mm planed
- The reduction is typically 3 to 5mm per face
Always measure what you are buying. Designing to nominal sizes and building with actual ones produces gaps.
The terms
Sawn, or rough sawn. As cut, unplaned. The nominal size, roughly. Rough surface, for structural and hidden work.
PAR, planed all round. Planed on all four faces. Smooth, smaller than nominal, for visible work.
PSE, planed square edge. Planed with square edges rather than rounded.
CLS, Canadian lumber standard. Planed with slightly rounded edges, dried and regularised. Common sizes are 38 x 63, 38 x 89 and 38 x 140mm. Widely used for stud walls, and the actual sizes are consistent, which is its advantage.
Regularised. Machined to a consistent depth, so joists sit level.
Kiln dried, KD. Dried in a kiln to a controlled moisture content. More stable and more expensive.
Air dried. Dried naturally. Slower, and generally to a higher moisture content.
Green. Freshly sawn and wet. It will shrink substantially.
Structural grading
Structural timber is graded for strength and marked accordingly.
- C16: the general structural grade, adequate for most domestic use
- C24: stronger, allowing longer spans or smaller sections
- The mark on the timber shows the grade, the species, the drying method and the grading body
Where a drawing or a span table specifies a grade, use it. Substituting C16 where C24 is specified reduces the load capacity.
Span tables in the Building Regulations guidance give permitted spans for each grade and size. Structural work is notifiable and should be checked against them.
Joinery grades
Graded for appearance rather than strength.
- Unsorted: the better quality, with fewer and smaller knots
- Fifths: lower quality, more knots and defects
- Merchants also use their own descriptions, so look at the actual timber
Moisture content
The single most important factor in whether timber stays where you put it.
- 8 to 12 per cent: interior, heated. Furniture, joinery, flooring in a heated house
- 12 to 15 per cent: interior, unheated or intermittently heated
- 16 to 20 per cent: exterior joinery
- Above 20 per cent: risk of fungal decay
Timber from a cold damp merchant's yard is wetter than a heated house. It will shrink after installation, opening joints and gapping floors.
Acclimatise for one to two weeks in the space where it will live, stickered so air reaches all faces.
The defects, and what they mean
Bow. A curve along the length, in the face. Sight along the board to spot it. Frequently pulls straight when fixed.
Spring, or crook. A curve along the length, in the edge. Harder to correct, and a real problem in a stud or a joist.
Cup. A curve across the width. Common in plain sawn boards. Can sometimes be planed out at the cost of thickness.
Twist, or wind. The board is not in one plane, so it rocks on a flat surface. The hardest defect to deal with and usually a reason to reject.
Knots. Where a branch met the trunk.
- Live or tight knots are bonded to the surrounding wood and generally acceptable
- Dead or loose knots can fall out, leaving a hole
- Knots weaken timber, especially near an edge or in a structural member
- Knots bleed resin through paint. Apply a knotting solution before priming
Shakes and checks. Splits along the grain. End checks are common and can be cut off. A shake running through the thickness is more serious.
Wane. The rounded edge of the log remaining on a corner, sometimes with bark. Reduces the usable section.
Blue stain. A fungal discolouration in sapwood. Mostly cosmetic and does not weaken the timber significantly, and it indicates the timber has been damp.
Step 1: choosing at the merchant
- Sight along every board from one end, looking for bow and spring
- Lay it on a flat surface and check for cup and rock
- Look at the end grain to see how it was cut
- Check for large or loose knots, particularly near edges
- Check for splits at the ends
- Reject anything twisted
- Ask before rummaging; most merchants are fine with it if you restack tidily
- Buy a little extra for defects and waste
Step 2: what to do with defects
- Use bowed boards where they will be fixed straight, such as noggins or short lengths
- Cut a long defective board into short pieces, since a defect over 3m may not matter over 500mm
- Position a board so a defect falls in the waste
- Turn a cupped board crown up when using it as a joist or a shelf
- Cut off end splits
- Set aside twisted timber for rough work
Step 3: common sizes
- Studwork: 38 x 63 or 38 x 89 CLS, or 50 x 75 and 50 x 100 sawn
- Joists: 47 x 100 up to 47 x 225, depending on the span
- Rafters: 47 x 100 to 47 x 175
- Battens: 25 x 38 or 25 x 50
- Skirting and architrave: sold by profile, commonly 18 or 20mm thick
- Standard lengths run in 300mm increments, commonly 1.8 to 4.8m
Buying a standard length is far cheaper than a cut length. Plan cutting lists around standard lengths.
If it goes wrong
Timber smaller than expected: nominal versus actual. Measure before designing.
Studs bowed after building: wet timber that dried. Use kiln dried, and let it acclimatise.
Knots showing through paint: apply knotting solution and reprime.
Floor gapped after a winter: the timber was not acclimatised before laying.
Joist not strong enough: check the grade and size against span tables, and get advice.