Most woodwork in older houses carries several layers of old gloss. New paint applied over it without keying will peel off in sheets, sometimes within months.
Test for lead first
Paint in properties built before 1992 may contain lead, and pre-1970s paintwork frequently does.
Use a lead paint test kit and test through the layers, since an old lead layer can sit under modern paint.
If lead is present, do not dry sand and do not use a heat gun. Use wet sanding or chemical stripper, wear a P3 respirator, keep children away, and collect all residue.
Sound lead paint that is not flaking is often safest overpainted rather than disturbed.
What you need
- Sugar soap or a degreaser, two buckets, sponges
- 180 grit abrasive, sanding block, sanding sponges for mouldings
- Adhesion primer suitable for glossy surfaces
- Undercoat and finish paint
- Filler and a filling knife
- Tack cloth
- P2 respirator, eye protection, dust sheets
Step 1: assess the existing paint
Push a fingernail or a scraper into it in a few places.
- Sound and firmly attached: key and overpaint
- Chipped or flaking in places: scrape back the loose areas and feather the edges
- Cracked, crazed or alligatored all over: strip it. Painting over crazing means the cracks reappear within a season
- So thick that detail is lost: strip it
Press masking tape onto the surface firmly and pull it off sharply. Paint coming away means the existing coat is not sound.
Step 2: degrease
Do this before sanding, not after.
Sanding a greasy surface drives the grease into the scratches you have just made, and the primer then bonds to grease.
- Wash with sugar soap solution, working over the whole surface
- Pay particular attention to door handles, the bottom of doors, and anywhere hands touch
- Rinse with clean water and a clean sponge
- Let it dry completely
- Run a dry hand over it. Any slipperiness means residue remains
Step 3: key the surface
The step that decides everything.
Sand the whole surface with 180 grit until the shine has gone uniformly.
That is the test: look along the surface at an angle towards a light. Any remaining shiny patch is a place the new paint will fail.
- Use a block on flat faces
- Use a sanding sponge on mouldings, which follows the profile
- Do not forget the edges, the top of the skirting, and the underside of anything
- Sand along the grain
Vacuum, then wipe with a tack cloth.
Step 4: fill
Now that the surface is sanded, defects are visible.
Fill dents, splits, old screw holes and chipped edges with fine surface filler, leave proud, sand flush with 180 and spot-prime.
Feather the edges of any area you scraped back, so there is no step.
Step 5: adhesion primer
Worth using in most cases and essential in some.
Use an adhesion primer when:
- Going from oil-based to water-based paint
- The existing surface is very hard, glossy or difficult to key fully
- Painting over a factory finish, melamine or a previously varnished surface
- You cannot sand into every corner and moulding
Apply one full coat and let it dry as the tin directs.
Step 6: undercoat and finish
Undercoat if you are changing colour or want the best finish, sanding it flat with 240.
Then two thin coats of finish, sanding lightly with 240 between them and wiping with a tack cloth.
Testing before doing the whole room
Where you are unsure about adhesion, do one small area first.
Prepare, prime and apply one coat to about 200mm of skirting. Leave it 48 hours.
Press masking tape onto it and pull off sharply. If the paint lifts, the preparation was not enough.
If it goes wrong
New paint peeling in sheets: not keyed, or not degreased. There is no fix except stripping back to a sound surface and starting again.
Paint lifting only around the handle: grease. Strip that area, degrease, prime and repaint.
Cracks reappearing: the underlying paint is crazed. It has to be stripped.
Finish looks lumpy: old build-up under the new paint. Strip, or accept a lower sheen finish.
Paint soft and never hardens: contamination, or incompatible products.
How much sanding is enough
The test is visual, not by time or effort.
Hold a light so it reflects off the surface at a shallow angle and look along it.
A properly keyed surface is uniformly matt with no bright patches. Shiny spots in the corners of mouldings are the usual failure, since that is where the block cannot reach.
Use a sanding sponge or fold abrasive over a shaped offcut to get into the profile.
When stripping is the better answer
- Paint so thick the mouldings have lost their shape
- Crazing or alligatoring across the surface
- Widespread flaking
- You want a clear or waxed finish
- A door has been painted shut repeatedly
How long it takes
Preparing the woodwork in an average room properly, washing, sanding, filling and priming, takes the best part of a day.
That is longer than applying the paint, and it is where the result is decided.
Varnished and stained woodwork
Painting over varnish or a stained finish needs the same approach plus a caution.
Sand thoroughly to key, then use an adhesion primer. Some stains and varnishes bleed through paint, so a shellac-based primer is the safer choice.
Test a small area and leave it 48 hours before committing to the whole job.