A clear or stained finish shows the timber, so every scratch, glue mark and sanding error is on display. There is nowhere to hide, unlike paint.
What you need
- Wood stain, water-based or spirit-based
- Wood conditioner or sanding sealer
- Varnish, polyurethane or acrylic, in your chosen sheen
- 120, 180, 240 and 320 grit abrasive
- A good synthetic brush, or a varnish brush
- Lint-free cloths and a tack cloth
- Gloves and eye protection
- Offcuts of the same timber for testing
Step 1: sand carefully
Sanding matters far more under a clear finish than under paint.
- Work up through the grits: 120, then 180, then 240
- Always sand along the grain. Cross-grain scratches are invisible on bare wood and glaringly obvious once stain goes on
- Do not skip more than one grade
- Use a block on flat surfaces
- Remove every trace of old glue, since glue blocks stain and shows as a pale patch
- Vacuum and wipe with a tack cloth
Do not sand beyond 240 before staining. Too fine a surface will not absorb the stain evenly.
Step 2: test on an offcut
Always. Stain looks completely different on different timbers, and on the same timber at different ages.
Test on an offcut of the same wood, sanded to the same grit, and let it dry fully.
Apply the varnish over the test too, since varnish deepens the colour noticeably.
Step 3: condition the wood
The step that prevents blotching.
Softwoods such as pine, and some hardwoods including birch and cherry, absorb stain unevenly, giving a patchy, blotchy result. The end grain and the softer growth rings drink far more.
Apply a wood conditioner or a thinned coat of sanding sealer, let it soak in for the stated time, and wipe off the excess.
Stain within the window the conditioner specifies, usually within a couple of hours.
This partially seals the absorbent areas so the stain takes evenly.
Step 4: apply the stain
- Stir it thoroughly. Pigment settles
- Apply generously with a brush or a cloth, working along the grain
- Work in manageable sections and keep a wet edge
- Let it stand for the time in the instructions, typically a few minutes. Longer means darker
- Wipe off the excess with a clean lint-free cloth, along the grain
- Wipe evenly and consistently, since this is what controls the final depth
Apply a second coat for a deeper colour once the first is dry, rather than leaving the first on longer.
Pay attention to end grain, which soaks up far more and goes much darker. Seal it first with conditioner.
Step 5: seal, then varnish
Let the stain dry fully, which may be 24 hours for a spirit-based stain.
Apply a sanding sealer or a thinned first coat of varnish, which seals the stain and stops the next coat lifting it.
Step 6: apply the varnish
- Stir gently. Do not shake, which whips in air bubbles that dry into the finish
- Decant into a kettle rather than working from the tin
- Load the brush lightly
- Apply along the grain in even strokes
- Lay off with the tips of the bristles in one direction and stop
- Do not overbrush, which creates bubbles and marks
- Keep the coats thin
Step 7: denib between coats
Essential for a smooth clear finish.
When each coat is fully hard, sand lightly with 320 grit or a fine abrasive pad, just enough to knock off the raised fibres and dust nibs.
The surface should feel completely smooth.
Vacuum and wipe with a tack cloth.
Three coats gives a durable finish; a floor or a worktop needs more.
Sheen and type
- Polyurethane: hard and durable, ambers slightly over time
- Acrylic or water-based: clear and non-yellowing, dries fast, less hard
- Matt, satin and gloss: gloss is the most durable and shows the most; satin is the usual choice
If it goes wrong
Blotchy stain: no conditioner on absorbent timber. Sand back to bare wood, condition, and restain.
Pale patches: glue residue or polish on the surface. Sand back and reapply.
Streaky stain: excess not wiped off evenly. Restain and wipe consistently along the grain.
Bubbles in the varnish: the tin was shaken, or the brush was overworked. Denib and apply a thin coat without overbrushing.
Varnish milky: applied in damp or cold conditions. Let it dry and recoat in better conditions.
Cross-grain scratches showing: sanded across the grain. There is no fix except sanding back and starting again.
Oil finishes as an alternative
Danish oil, tung oil and hardwax oils penetrate rather than forming a surface film.
- Easier to apply: wipe on, leave, wipe off the excess
- Easy to repair in patches, unlike varnish, which has to be sanded back
- Less protective against water and wear
- Need reapplying periodically
Oil-soaked rags can self-ignite. Lay them out flat outdoors to dry, or soak them in water, before disposal. Never leave them in a pile or a bin.
How long it takes
Sanding through the grits is the slow part, and it cannot be rushed under a clear finish.
A door takes half a day to sand, an hour to stain, and three coats of varnish over three days with denibbing between.
Working conditions
- Varnish shows dust more than paint, so vacuum the room first and do not sweep
- Work at a moderate temperature with gentle ventilation
- Avoid draughts, which carry dust onto the wet surface
- Do not apply in high humidity, which can turn varnish milky