Back to Repairs

Fixing Uneven and Bumpy Walls

Fixing Uneven and Bumpy Walls
DIY Guides Editorial 9 March 2026

Most walls in older houses are not flat. Whether that matters depends on what is going on them, so measure before deciding on a remedy.

Step 1: measure how bad it is

  1. Hold a long straight edge, 1.8m or 2m, against the wall vertically
  2. Note the size of any gap behind it, using a tape or a coin as a gauge
  3. Repeat horizontally and diagonally, across the whole wall
  4. Mark the high spots and the hollows in pencil
  5. Note the worst deviation

A rough guide to what matters:

  • Under 3mm over 2m: effectively flat. Fine for anything
  • 3 to 5mm: fine for paint and wallpaper, marginal for large tiles
  • 5 to 10mm: visible under raking light, and a problem for tiling and for sheen paint
  • Over 10mm: needs correcting before most finishes

Step 2: work out what it needs to take

  • Matt paint: very forgiving. Minor unevenness is barely visible
  • Sheen or silk paint: unforgiving. Raking light shows everything
  • Wallpaper: hides small imperfections, highlights ridges and hollows
  • Small tiles: tolerate a certain amount
  • Large-format tiles: tolerate almost nothing, since a rigid tile cannot follow a curve and the corners lip
  • Panelling: can be packed out to a straight line

A wall that is fine for a matt painted bedroom may be unusable for large tiles.

Option 1: fill and sand

For localised bumps and hollows rather than a generally wavy wall.

  1. Knock off any high spots: plaster nibs, paint runs, old adhesive
  2. Sand high areas back with 80 or 120 grit on a block
  3. Fill hollows with powder filler, in layers no thicker than the packet allows
  4. Rule off with a straight edge held across the sound wall each side
  5. Sand flush and feather well out
  6. Recheck with the straight edge
  7. Spot-prime the repairs

Practical up to about 5mm of correction over a limited area. Beyond that it becomes an enormous amount of sanding.

Option 2: skim the wall

A plasterer applies a thin coat over the whole wall, giving a flat surface.

  • Corrects: up to about 5mm, more with a bonding coat underneath
  • Time: a day for a room, plus around four weeks drying
  • Result: the best finish available
  • The usual answer where the wall needs to be genuinely flat

Skimming is a skilled trade and rarely worth attempting for the first time on a whole wall.

Option 3: cross-line it

Lining paper hung horizontally, then painted.

  • Corrects: minor texture, pitting and hairline cracking. Not real unevenness
  • Time: a day, plus drying
  • Cost: low
  • Use a heavier grade, 1400 or above, to bridge more

Lining paper disguises a poor surface. It does not make a wavy wall straight.

Option 4: overboard it

Plasterboard fixed over the existing wall, then skimmed.

Dot and dab: boards bedded onto dabs of adhesive, which are adjusted to bring every board into the same plane.

Battened: timber battens fixed to the wall and packed to a straight line, with boards screwed to them. Better where the wall is very uneven or damp is a factor, since it leaves a cavity.

  • Corrects: almost anything, since the board is set to a line rather than following the wall
  • Time: a day or two, plus skimming and drying
  • Cost: more than skimming, and the definitive answer
  • Costs 25 to 50mm of room width depending on the method

Which to choose

  • A few bumps, matt paint: fill and sand
  • Generally poor surface, painting: skim, or cross-line if the budget is tight
  • Tiling, especially large format: skim or overboard. Do not tile onto an uneven wall
  • Very uneven, or damp involved: overboard on battens
  • Period house where you want to keep the character: accept some unevenness and use matt paint

Practical points

  • Check the wall again after any correction, with the same straight edge
  • Overboarding and skimming both affect skirting, architrave, sockets and door frames
  • Sockets need extending forward with a spacer if the wall is thickened
  • Skirting may need removing and refitting
  • Allow four weeks for new plaster to dry before painting

If it goes wrong

Still uneven after filling: too much correction attempted with filler. It needs skimming.

Tiles lipping: the wall was not flat enough for the tile size.

Lining paper following the bumps: expected. Paper disguises texture, not shape.

Sockets recessed after overboarding: fit box extenders.

Repairs visible under sheen paint: use matt, or skim the wall.

How much correction each option gives

  • Filling: up to about 5mm, over a limited area
  • Skim: up to about 5mm across a whole wall
  • Bonding coat and skim: up to about 15mm
  • Dot and dab overboarding: up to about 25mm
  • Battened overboarding: effectively unlimited, since the battens are packed to a line

How long each takes

  • Filling and sanding: a day, plus drying
  • Cross-lining: a day, plus a day of drying
  • Skimming: a day, plus four weeks of drying
  • Overboarding and skimming: two to three days, plus four weeks

Accepting an old wall

In a period house, perfectly flat walls can look wrong.

Slight undulation is part of what an old building looks like, and matt paint on a gently uneven wall reads as character rather than as a fault.

Correct what will cause a practical problem, such as a wall being tiled, and leave the rest.

A summary

  1. Measure with a long straight edge before deciding anything
  2. Judge it against what the wall has to take
  3. Fill and sand for localised defects only
  4. Skim or overboard where the wall must be genuinely flat
  5. Never tile onto an uneven wall